darraghbr/Prusa-MK3-Material-Profiles

Taulman Alloy 910 extrusion issues

Opened this issue · 0 comments

Currently I am struggling to get the Taulman Alloy 910 to print well, at some point in the print the extrusion quality goes downhill, the areas of poor extrusion appear to line up with areas of low mass flow rate, potentially indicating a blockage in the nozzle.

I suspect that the material is becoming annealed in the nozzle and is causing issues. I have tried aggressively drying the filament to no avail.